Smooth transparent amorphous layers based on a zinc-tin-oxide composite system
Akhmedov A. K.1, Murliev E. K.1, Abduev A. Kh.2,3, Asvarov A. Sh.1
1Amirkhanov Institute of Physics, Daghestan Federal Research Center, Russian Academy of Sciences, Makhachkala, Russia
2 Federal State University of Education, Mytishchi, Moscow region, Russia
3Russian Peoples’ Friendship University, Moscow, Russia
Email: cht-if-ran@mail.ru

PDF
Smooth amorphous oxide thin films were obtained by using rf magnetron sputtering of ceramic targets based on a mixture of zinc and tin oxides (ZTO). The influence of the target composition, oxygen content in the working gas, and film thickness on the morphology, structure, and optical characteristics of low-temperature deposited ZTO films has been studied. The minimum relief is observed in films obtained by sputtering a target with equal molar contents of zinc and tin oxides. When using this target, some polishing effect is found when the surface roughness of the Si substrate with an ultrathin ZTO layer (up to 15 mm of thickness) is less than that of the original Si substrate.. Keywords: Zinc Oxide, Tin Oxide, Thin Film, Magnetron Sputtering, Growth.
  1. W. Kim, S. Kang, Y. Lee, S. Mun, J. Choi, S. Lee, C.S. Hwang, J. Mater. Chem. C, 11, 8254 (2023). DOI: 10.1039/d2tc05090k
  2. C.H. Kim, Y.S. Rim, H.J. Kim, J. Phys. D: Appl. Phys., 47, 385104 (2014). DOI: 10.1088/0022-3727/47/38/385104
  3. M. Shaji, K.J. Saji, M.K. Jayaraj, Mater. Sci. Semicond. Process., 150, 106927 (2022). DOI: 10.1016/j.mssp.2022.106927
  4. S.B. Pagar, T.N. Ghorude, M.D. Deshpande, K.S. Kannan, J. Inorg, Organomet. Polym. Mater., 33, 2752 (2023). DOI: 10.1007/s10904-023-02650-8
  5. F. Turkoglu, H. Koseoglu, M. Ekmekcioglu, A. Cantas, G. Aygun, L. Ozyzer, J. Mater. Sci: Mater. Electron., 33, 10955 (2022). DOI: 10.1007/s10854-022-08075-2
  6. N.M. Martin, T. Torndall, M. Babucci, F. Larsson, K. Simonov, D. Gaidek, L.R. Merte, H. Rensmo, C. Platzer-Bjorkman, ACS Appl. Energy Mater., 5, 13971 (2022). DOI: 10.1021/acsaem.2c02579
  7. M. Morales-Masis, F. Dauzou, Q. Jeangros, A. Dabirian, H. Lifka, R. Gierth, M. Ruske, D. Moet, A. Hessler-Wyser, C. Ballif, Adv. Funct. Mater., 26, 384 (2016). DOI: 10.1002/adfm.201503753
  8. D.L. Young, D.L. Williamson, T.J. Coutts, J. Appl. Phys., 91, 1464 (2002). DOI: 10.1063/1.1429793
  9. A.Sh. Asvarov, A.E. Muslimov, A.K. Akhmedov, V.M. Kanevsky, Coatings, 10, 1076 (2020). DOI: 10.3390/coatings10111076
  10. I. Sieber, N. Wanderka, I. Urban, I. Dorfel, E. Schierhorn, F. Fenske, W. Fuhs, Thin Solid Films, 330, 108 (1998). DOI: 10.1016/s0040-6090(98)00608-7

Подсчитывается количество просмотров абстрактов ("html" на диаграммах) и полных версий статей ("pdf"). Просмотры с одинаковых IP-адресов засчитываются, если происходят с интервалом не менее 2-х часов.

Дата начала обработки статистических данных - 27 января 2016 г.

Publisher:

Ioffe Institute

Institute Officers:

Director: Sergei V. Ivanov

Contact us:

26 Polytekhnicheskaya, Saint Petersburg 194021, Russian Federation
Fax: +7 (812) 297 1017
Phone: +7 (812) 297 2245
E-mail: post@mail.ioffe.ru